The surface state changes of titanium alloys during heat treatment and subsequent processing were systematically analyzed. The formation mechanism of oxide layer and oxygen-rich diffusion layer and their influence on pickling and removal process were analyzed. The applicable scope and combination strategies of different descaling methods were reviewed, aiming to provide a theoretical basis for formulating reasonable surface treatment process routes.

I. Necessity and Application Scenarios of Surface Treatment
Surface treatment is typically required after intermediate and final heat treatment processes for titanium and titanium alloys to achieve the following objectives:
1. Surface Cleaning: Removing metal oxide scale and various contaminants generated during high-temperature heating or processing.
2. Reducing Surface Activity: Minimizing the chemical activity of exposed metal surfaces to prevent contamination during subsequent processing or service.
3. Coating Pretreatment: Obtaining a suitable substrate surface condition through surface treatment before and during the application of protective or functional coatings (such as corrosion-resistant, high-temperature oxidation-resistant, and wear-resistant coatings) to enhance coating adhesion and service performance.
II. Formation Mechanism of Oxide Layer and Oxygen-Rich Diffusion Layer
The pickling conditions for titanium rods and their alloys mainly depend on the type and characteristics of their surface oxide layer and adjacent substrate reaction layer, both of which are significantly affected by the temperature history of high-temperature heating processes and hot working processes (such as forging, casting, and welding).
• Low-temperature or short-duration heating (below approximately 600℃): Only a thin oxide film forms on the surface. This film has a relatively loose structure and can generally be dissolved and removed by conventional acid pickling.
• High-temperature heating (above approximately 600℃): Not only does a thicker, dense oxide layer form, but an oxygen-rich diffusion zone (i.e., an oxygen-stabilized α layer) is also generated beneath it. This diffusion layer has high hardness, low plasticity, and relatively stable chemical properties. It must be completely removed by acid pickling; otherwise, it will seriously affect subsequent processing and product service life.
III. Commonly Used Oxide Scale Removal Methods
For oxide layers of different thicknesses and structures, the following three types of descaling methods are mainly used in industry:
1. Mechanical Descaling: Suitable for removing thicker original oxide scale and hard surface layers. Methods such as sandblasting, shot peening, or grinding can be used. This method is highly efficient, but it is difficult to completely remove the microscopic oxygen-rich layer on the substrate surface when used alone.
2. Molten Salt Bath Descaling: The workpiece is immersed in high-temperature molten salt (such as alkaline boiling), where the oxide scale is loosened and peeled off through chemical melting. This method is highly effective for removing thick oxide scale from complex-shaped workpieces.
3. Acid Pickling Descaling: Oxide scale and oxygen-rich layer are removed through chemical dissolution in an acid solution (usually a mixture of HF and HNO₃). This method yields a clean, bright metal surface with low reactivity.
IV. Process Combination Strategies and Selection Principles
In actual production, a single method often fails to balance efficiency and quality; therefore, combined processes are frequently employed:
* Conventional Combination Route: For oxide layers formed at medium to low temperatures, a combination of "mechanical descaling (optional) + acid pickling" or "molten salt bath + acid pickling" is typically used. This involves first mechanically or through a salt bath to break down and remove most of the outer oxide scale, followed by acid pickling to dissolve the remaining oxide layer and oxygen-rich diffusion layer, resulting in a uniform and clean surface.
• High-temperature oxide layer treatment: For dense oxide layers and diffusion layers formed by heating at temperatures above 600℃, a highly corrosive molten salt bath pretreatment is generally required, followed by acid pickling. However, for some thinner oxide layers formed by brief heating at around 600℃, if their structure is not dense, they can be removed directly using a conventional acid pickling process in one step.
Contact Us
Shaanxi Mingtai Dingsheng Metal Material Co., Ltd
Medical Titanium Alloy Materials | Bar, Plate, Wire, Disc & Powder
Tel: +86 17391509251
Email: Kristy@mt-titanium.com
Address: Room 103, Building 53, Gaoyi Industrial Park, Baqiu Town, High-tech Development Zone, Baoji City, Shaanxi Province, China