Medical Grade Titanium Plate for Joint Replacement

Send Inquiry
Medical Grade Titanium Plate for Joint Replacement
Details
Material: Ti-6Al-4V ELI (Grade 23) / CP Grade 2 / CP Grade 4
Standard: ASTM F136 / ASTM F67
Thickness: 1.0mm – 8.0mm
Width: 10mm – 60mm
Length: 50mm – 300mm
Surface: Polished, anodized, or plasma spray coated
Category
Medical Titanium Plate
Share to
Description

What it is

 

 

Knee replacement. Hip replacement. Shoulder. Ankle. The joint is worn out. Cartilage gone. Bone rubbing on bone. Surgeon cuts the bone and puts in an implant.
The raw material for those implants is what we're talking about here. Tibial trays. Femoral components. Acetabular shells. Glenoid bases.
The plate gets machined. Cut. Drilled. Shaped. Coated. Becomes the part that goes into the patient.

 

Our Products

ASTM F67 pure titanium plate
 
Gr23 titanium plate
 
plate 5
 

 

Titanium vs cobalt chrome vs stainless

 

 

Joint replacements used to be mostly cobalt chrome or stainless steel. Still are, in some cases.
But titanium took over many applications.
No nickel. Cobalt chrome has cobalt and chromium. Stainless has nickel. Titanium has neither. Better for allergy-prone patients.
Better bone integration. Titanium forms an oxide layer. Bone grows to it. Cobalt chrome doesn't.
Lighter. Titanium is about half the weight of cobalt chrome. Patient feels the difference.
MRI compatible. Cobalt chrome causes artifact. Titanium doesn't.
For joint replacement plates, the choice is clear for most components. Ti-6Al-4V ELI for strength. CP titanium for coatings.
 

Which grade for which joint component

 

 

Component Grade Why
Tibial tray (knee) Grade 23 ELI High strength. Thin profile.
Femoral component Grade 23 ELI or CoCr Titanium or cobalt. Surgeon preference.
Acetabular shell (hip) Grade 2 or Grade 4 Bonding surface. Porous coating applied.
Glenoid base (shoulder) Grade 23 ELI Small. Needs strength.
Augments and wedges Grade 23 ELI Structural. Load bearing.
Cementless fixation plate Grade 2 or Grade 4 Pure titanium. Easy to coat.

Different grades for different jobs. Grade 23 ELI for strength. Grade 2 or Grade 4 for pure titanium coating applications.
 

Material specs

 

 

Property Grade 23 ELI Grade 4 CP Grade 2 CP
Standard ASTM F136 ASTM F67 ASTM F67
Tensile (min) 860 MPa 550 MPa 345 MPa
Yield (min) 795 MPa 483 MPa 275 MPa
Elongation ≥ 10% ≥ 15% ≥ 20%
Density 4.43 g/cm³ 4.51 g/cm³ 4.51 g/cm³

 

How it becomes a joint implant

 

 

Plate arrives at the implant manufacturer. First step - cut the shape. Waterjet or laser. Rough outline of a tibial tray or acetabular shell.
Then CNC machining. Five-axis mills. Pocketing. Drilling. Threading. Creating the locking mechanism for the polyethylene insert.
Surface treatment. Polishing where bone doesn't grow. Coating where bone should attach. Plasma spray. Porous coating. Hydroxyapatite.
Final cleaning. Sterilization. Packaging.
Every joint replacement plate starts as a flat plate. The rest is machining.
 

Tibial tray - the main application

 

 

Knee replacement. The tibial tray sits on top of the shin bone. Holds the plastic bearing. Takes load with every step.
Tray is thin. 3mm to 5mm. But strong. Has to support body weight. Has to lock the insert in place.
Tibial trays are almost always Grade 23 ELI. 860 MPa tensile. Can be thin and still strong.
The plate has pegs or a stem on the underside. Goes into the bone. Cut from the same plate. Machined from solid.
 

Acetabular shell - the hip application

 

 

Hip replacement. The acetabular shell goes into the pelvis. Replaces the worn socket.
Shell is curved. Starts as a flat plate. Stamped or machined into a dome shape.
Surface needs porosity. Bone grows into porous coating. Locks the shell in place.
Shells are usually Grade 2 or Grade 4. Pure titanium. Takes the porous coating well. Coating goes on both sides or just the bone side.
 

Surface coatings for bone ingrowth

 

 

Joint replacements need to stay put. Cemented or cementless.
Cementless relies on bone growing into the implant surface. That requires a coating.
Plasma spray. Titanium powder sprayed onto the plate surface. Creates rough, porous layer. Pores are 100-300 microns. Bone grows in.
Porocoat. Beaded surface. Small titanium beads bonded to the plate.
Trabecular metal. Tantalum. More expensive. Used in some hip and knee systems.
The base plate needs to be clean. No oxide. No contamination. Coating won't stick to dirty metal.
We supply plate with your specified surface preparation. Pickled. Grit blasted. Ready for coating.
 

Machining considerations

 

 

Joint implant machining is high precision. Tolerances in microns. Five-axis CNC. Hard materials.
Ti-6Al-4V ELI machines like any titanium. Slow speeds. Carbide tools. Flood coolant. Don't let the tool rub.
CP titanium (Grade 2, Grade 4) is softer. Easier to machine. Gummy. Watch out for built-up edge.
We supply plate blanchard ground or fly cut. Flat. Parallel. Ready for your machining center.
 

Traceability

 

 

Joint replacements are Class III medical devices. Highest risk category. Highest regulatory scrutiny.
Every plate comes with full traceability.
Heat number. Mill test report. ASTM F136 or F67 cert. Chemical analysis. Mechanical test results. Grain size if specified.
EN 10204 3.1 standard. 3.2 with third-party witness.
We retain samples from every heat. If your notified body shows up for an audit, we have the backup.
 

RFQ

 

 

Q: Grade 23 ELI or Grade 4 for tibial tray? 

A: Grade 23 ELI. Tibial tray takes full body weight. Need high strength. Grade 4 pure titanium is 550 MPa. Too weak for thin tray designs.

Q: What thickness for a tibial tray blank? 

A: 3mm to 5mm. Depends on design. Small size needs thinner. Large size needs thicker.

Q: What surface finish for coating? 

A: Grit blasted or pickled. Remove oxide. Create anchor profile for the coating. Polished surface is too smooth. Coating won't stick.

Q: Do you supply plate with porosity? 

A: No. We supply solid plate. You apply porous coating. Coating process is implant manufacturer's proprietary technology.

Q: What certifications come with the plate? 

A: ASTM F136 or F67 cert. MTR with heat number. Mechanicals. EN 10204 3.1. 3.2 available.

Q: Lead time? 

A: Stock thicknesses ship in 7-10 days with paperwork. Non-stock sizes take 3-5 weeks.

Q: Packaging for clean room? 

A: Individual plastic sleeves. Sealed. Labels show material, thickness, lot number, heat number, ASTM spec.

Q: Cut to rough shape? 

A: Yes. Send DXF or DWG. Waterjet or laser cut. Deburr. Pack. Minimum order applies.

 

 

Bottom line

 

 

Joint replacement implants need strong, biocompatible material. The right titanium plate delivers that.
Grade 23 ELI for tibial trays, glenoid bases, augments. Grade 2 or Grade 4 for acetabular shells and coating substrates.
ASTM F136 or F67. Full traceability. Flat. Parallel. Ready for machining and coating.
From knee to hip to shoulder.
 

Contact

 

 

 

Need a quote on medical grade titanium plate for joint replacement? Tell us which component, grade, thickness, width, length, and quantity. Include any surface finish or coating prep requirements. We'll reply within 24 hours.

Email: kristy@mt-titanium.com

WhatsApp: +86-17391509251

 

 

Hot Tags: medical grade titanium plate for joint replacement, China medical grade titanium plate for joint replacement manufacturers, suppliers, factory, Craniofacial Reconstruction Titanium Plate ASTM F67, Medical Grade Titanium Plate for Joint Replacement, Minimally Invasive Surgery Titanium Fixation Plate, Orthopedic Trauma Titanium Plate, Ti 6Al 4V ELI Medical Plate for Surgical Implants, Titanium Bone Plate

Send Inquiry